Dick,

I was told to mig the inside and the clean up with grinder--the to braze-solder 
the outside joint using a 3/16 or 1/8 fluxed rod--ie use low heat small gas 
tip, heat the flange and let the metal flow into the tube - flange joint 
crack--if the metal bubbels you are using to much heat. wmts 
> 
 
> 