Phosphoric acid - I get mine from body shop suppliers. It's called
metal prep. Usually it has to be diluted 50%. I may have used it
straight from the bottle and experimented with soak time.  Did not
harm the plastic.

Mike L
60A,67E,59Bug


----- Original Message -----
From: Larry Hoy <larryhoy@prodigy.net>
To: Michael Lupynec <mlupynec@globalserve.net>;
<mgs@autox.team.net>
Sent: May 16, 2001 10:22 AM
Subject: RE: Fused circuits & connectors


> Mike, were do you find phosphoric acid?
>
> What will it do to the rubber insulators?

///