Part has to be baked at moderate temperature for a couple of hours, and 
most important, the process has to begin as soon as it's out of the plating 
tank. If the part is allowed to sit for just 24 hours without treatment, 
the part will be compromised.

Does anyone happen to have a metallurgy specification for torsion bars?

Mike Frank

At 08:20 AM 11/14/02, lwdent wrote:
>Suffice it to say in initials a slow heat for a number of hours to
>remove any hydrogen trapped under the plating, as I recall.