A PO of my 3A brazed a few small mild steel patches that are acceptable. I
need to do some metal fill at the edge of one of the patches and am hesitant
to braze as I am afraid that the heat will cause the existing braze to let
go. Does anyone know if tin/copper lead free solder on a roll (plumbing) with
no flux core is the same that is sold as lead free body solder? I don't need
much so I am not too excited about buying body solder.
Body filller is not an acceptable soluton as there are pin holes that need
to be filled and I do not like to fill holes with filler.
David Lylis
69 TR6 CC26160L
60 TR3A TS74461LO
**************Ideas to please picky eaters. Watch video on AOL Living.
(http://living.aol.com/video/how-to-please-your-picky-eater/rachel-campos-duffy/
2050827?NCID=aolcmp00300000002598)
_______________________________________________
Support Team.Net http://www.team.net/donate.html
This list supported in part by the Vintage Triumph Register
http://www.vtr.org
Triumphs@autox.team.net
http://autox.team.net/mailman/listinfo/triumphs
http://www.team.net/archive
|