I have just had the first experience with the nickel plating kit from
Eastwood. Well... I do not know much confidence I have in my plated
parts. Actually, there was kind of a orangy tone on some of the parts
when they dried.
I had heard some quite positive comments regarding this set on the
list. I would like to know how you guys are cleaning your parts
before plating. And what lenght of time you leave the parts in the
bath. (I am using a power supply in place of the 2 D batteries, with
gives typically 1.6 amps at 1.5V. I do not know what kind of current
to voltage you would have with the batteries)
More controversial: Given what you get for your buck at Eastwood, I
wonder if some home platers do go to the local plating shop to
purchase the electrolyte and the nickel electrodes.
Have a nice day.
Francois
TR3A,TR3B
Get email alerts & NEW webcam video instant messaging with Yahoo! Messenger
/// triumphs@autox.team.net mailing list
/// To unsubscribe send a plain text message to majordomo@autox.team.net
/// with nothing in it but
///
/// unsubscribe triumphs
///
|