the temp. is not high enough to effect the tensile strength.  Now if you got
the temp above 1500 F. you would run into a tempering problem.

Larry Zink
1964 Spitfire4 Mk1
Houston,Texas
-----Original Message-----
From: Gano, Ken <kengano@advant.com>
To: triumphs mail list <triumphs@autox.team.net>; shop talk
<shop-talk@autox.team.net>
Date: Wednesday, May 20, 1998 11:17 PM
Subject: hot bolts?


>
>Would powder coating the heads of bolts (400 degrees F., 15 minutes) have
>any adverse effect on the strength of grade 5 or grade 8 bolts?  I wouldn't
>think so, but am just curious.
>
>kengano@advant.com