Actually after 16 years in the business we have had only two incidents in
which the coating has caused any difficulty. If this is a concern we will
mask off the area in question. The thickness obtained is a function of the
application process and can vary from person to person and the curing temp.
used. Cermakrome is much more flexible than most people realize, but baking
it at 700 to 800 hundred degrees increases the chance of the application
interfering with fit.
It all comes down to the preparation and the amount of expertise of the shop
doing the job.
Sean
Caps Bright Hot Coatings/Powder Coatings
|