Speaking of welding supplies and such.... I just tried something that worked
fairly well...
When I weld Steel the tip always gets stuck in the puddle ( cause my hand
control isn't as good as it could be )... and since that's been happening I've
had a tendency to keep the tungsten fairly close into the cup....
I've gotten a bit better at welding over the last few years and thought I'd
try sticking the tungsten out farther and increasing the argon flow just a
bit... On my welder this seems to be about 4lbs higher at 24 now..... With a
sharp tip I can finally weld a smaller bead...
One of you is going to beat me up for not learning this earlier... but you
know what that's why they call it practicing.....
Keith ( Life is GOOD )
|