Thanks Neil,
God--I feel so inaddaquite and have sooooo much to LEARN--I guess thats why we 
are called rookies  wmts
> 
> > 
> If it bubbles, you've used WAY too much heat. This forms intermetallics and
> that joint becomes brittle & weak. Use a moderate sized gas tip so that the
> heat is spread over a fairly good-sized area; if you use a tiny tip and
> crank up the heat, it is concentrated onto the filler rod and the
> overheating causes "fuming" (bubbling).
> 
> Regards, Neil     Tucson, AZ
> 
> 
> 
> Dick,
> 
> I was told to mig the inside and the clean up with grinder--the to
> braze-solder the outside joint using a 3/16 or 1/8 fluxed rod--ie use low
> heat small gas tip, heat the flange and let the metal flow into the tube -
> flange joint crack--if the metal bubbels you are using to much heat. wmts 
> > 
>  
> > 
> 
>   "Sparky"
> Lakester 2211
> 

  "Sparky"
Lakester 2211

///  unsubscribe/change address requests to majordomo@autox.team.net  or try
///  http://www.team.net/mailman/listinfo
///  Archives at http://www.team.net/archive/land-speed
///  what is needed.  It isn't that difficult, folks.


<Prev in Thread] Current Thread [Next in Thread>
  • Re: RE: Header welding--ROOKIE, wmtsmith <=