Good to know, thank you Ken!
I ordered .027 and .030 in 12"x39" sheets from RotoMetals.
Mix and match. I will use the leftovers for zinc plating.
John
At 12:34 AM 12/17/2010 +0000, you wrote:
>John
>The tin I used for my spring rebuild mikes .025 inch thick
>Ken Mason
>
> > Date: Thu, 16 Dec 2010 08:54:24 -0800
> > From: jmsdarch@sbcglobal.net
> > Subject: [Healeys] Leaf spring interleaves
> >
> > Does anyone know the correct thickness for the zinc interleaves? I
> > mic .027 to .030. Both thickness appear to be available on the market.