As far as chrome embrittling steel components, it can happen. The parts must undergo a low temp heat treatment to avoid hydrogen embrittlement. It is just one more thing to worry about with chrome platting (and some nickel). Thanks to all who responded about the Zinc. I'm going to try some local platting shops first to see what they will charge. Joe(B) Only $9.95 per month! |