Hello all,
The consensus seems to be yellow zinc. Since I already get lots of
carb parts done I'll clean it up and put it in with the next batch
keith
>
>
> I've got a 2L heat shield that I would like to restore to its original
> finish.
>
> Call your local platers and find who does zinc plating with zinc chromate
> conversion finnish.
> Take your heat shield, washer bracket, coil bracket, hood latch medalion,
> hood latch, relay covers, voltage regulator cover, Alternator pulley/fan,
> every 8mm nut that uses a 12mm wrench, throtle cable standoff, throtle cam
> and pivot bolts, carb center linkage, front manifold water pipe, horns (in
> pieces), top timing chain cover, feul hose bracket, engine lift brackets,
> any and all old style hose clams, radiator cap, oil pressure tube-to-hose
> bracket and oil dip stick.
>
> wire brush any rust off, sand smooth for that just like new finish. They
> charge by the pound and youv'e got 3 maybe 4 pounds. Most cases, these guys
> are really quick, they might do it while you wait.
>
> When you lift your hood, and all that cold cad glitters in the sun, and all
> the other roadster owners go "ooohhh"
Return-Path: <datsun-roadsters-owner@autox.team.net>
Received: from rly-zd01.mx.aol.com (rly-zd01.mail.aol.com
[172.31.33.225]) by air-zd03.mail.aol.com (v81.9) with ESMTP id
MAILINZD33-1005112207; Fri, 05 Oct 2001 11:22:07 -0400
Received: from teamfat2.dsl.aros.net (teamfat2.dsl.aros.net
[207.173.21.42]) by rly-zd01.mx.aol.com (v80.21) with ESMTP id
MAILRELAYINZD110-1005112145; Fri, 05 Oct 2001 11:21:45 2000
Received: (from majordom@localhost) by teamfat2.dsl.aros.net
(8.11.0/8.11.0) id f95FIj923444 for datsun-roadsters-actors; Fri, 5
Oct 2001 09:18:45 -0600 (MDT)
Message-ID: <48506CC52C52D3119B4300508B0903B501EE0180@EXCHANGE10>
From: "Laury, Victor" <LauryV@MTA.NET>
To: "'Keith0alan@aol.com'" <Keith0alan@aol.com>,
datsun-roadsters@autox.team.net
Subject: RE: 2000 heat shield ?
Date: Fri, 5 Oct 2001 08:16:10 -0700
MIME-Version: 1.0
X-Mailer: Internet Mail Service (5.5.2650.21)
Sender: owner-datsun-roadsters@autox.team.net
Precedence: bulk
Reply-To: "Laury, Victor" <LauryV@MTA.NET>
I've got a 2L heat shield that I would like to restore to its original
finish.
Call your local platers and find who does zinc plating with zinc chromate
conversion finnish.
Take your heat shield, washer bracket, coil bracket, hood latch medalion,
hood latch, relay covers, voltage regulator cover, Alternator pulley/fan,
every 8mm nut that uses a 12mm wrench, throtle cable standoff, throtle cam
and pivot bolts, carb center linkage, front manifold water pipe, horns (in
pieces), top timing chain cover, feul hose bracket, engine lift brackets,
any and all old style hose clams, radiator cap, oil pressure tube-to-hose
bracket and oil dip stick.
wire brush any rust off, sand smooth for that just like new finish. They
charge by the pound and youv'e got 3 maybe 4 pounds. Most cases, these guys
are really quick, they might do it while you wait.
When you lift your hood, and all that cold cad glitters in the sun, and all
the other roadster owners go "ooohhh"
Victor
70 SRL 31113136
72 HLS30 48255
65 L-320 Pickup
Los Angeles
http://albums.photopoint.com/j/AlbumList?u=123073
SoCalROC http://www.socalroc.com/
///
/// datsun-roadsters@autox.team.net mailing list
///
///
/// datsun-roadsters@autox.team.net mailing list
///
|